RR2Ce-1・RR5Ce-1・RR10Ce-1
Others
With product properties data and TEM images.
Differences between Ce-1 and Ce-2
Ce-1
- BET surface area = 114㎡/g
- CO oxidation = 44℃(50% conversion)
- Glucose oxidation in liquid phase = 0% conversion for 1 h
- Au is supported as Au³⁺
Ce-2
- BET surface area = 20.4㎡/g
- CO oxidation = 54℃(50% conversion)
- Glucose oxidation in liquid phase = 11% conversion for 1 h
Product(No.) | RR2Ce-1 | RR5Ce-1 | RR10Ce-1 |
---|---|---|---|
Net weight(g) | 2g | 5g | 10g |
Price All prices excluded tax. |
26,000 yen | 56,000 yen | 93,000 yen |
Gold loading to support | 1wt% | ||
---|---|---|---|
Support | CeO₂ | ||
Preparation method | DP(Deposition - Precipitation) | ||
Calcination temperature(℃) | 300 |
Free selectRequest for Quotation
Select FiveRequest for Quotation
RR2C・RR5C・RR10CC(KetjenBlack)
RR2Al・RR5Al・RR10AlAl₂O₃
RR2Si・RR5Si・RR10SiSiO₂
RR2Ti・RR5Ti・RR10TiTiO₂
RR2Mn・RR5Mn・RR10MnMnO₂
RR2Fe・RR5Fe・RR10FeFe₂O₃
RR2Co・RR5Co・RR10CoCo₃O₄
RR2Ni・RR5Ni・RR10NiNiO
RR2Zn・RR5Zn・RR10ZnZnO
RR2Zr・RR5Zr・RR10ZrZrO₂(Zirconia)
RR2Ce-1・RR5Ce-1・RR10Ce-1CeO₂
RR2Ce-2・RR5Ce-2・RR10Ce-2CeO₂